Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch tensile/fracture test data for P92 nt material at -79 °C and a displacement rate of .00833 mm/s Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. For estimating the tensile properties a series of tests were carried out at room temperature on Gr. 91 steel with different hea... WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch tensile/fracture test data for P92 nt material at -120 °C and a displacement rate of .00833 mm/s Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. For estimating the tensile properties a series of tests were carried out at room temperature on Gr. 91 steel with different hea... WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch tensile/fracture test data for P92 nt material at -183 °C and a displacement rate of .00833 mm/s Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. For estimating the tensile properties a series of tests were carried out at room temperature on Gr. 91 steel with different hea... WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch tensile/fracture test data for P92 nt material at -94 °C and a displacement rate of .00833 mm/s Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. For estimating the tensile properties a series of tests were carried out at room temperature on Gr. 91 steel with different hea... WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch tensile/fracture test data for P92 nt material at -168 °C and a displacement rate of .00833 mm/s Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. For estimating the tensile properties a series of tests were carried out at room temperature on Gr. 91 steel with different hea... WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch tensile/fracture test data for P92 nt material at -110 °C and a displacement rate of .00833 mm/s Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. For estimating the tensile properties a series of tests were carried out at room temperature on Gr. 91 steel with different hea... WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch tensile/fracture test data for P92 nt material at -98 °C and a displacement rate of .00833 mm/s Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. For estimating the tensile properties a series of tests were carried out at room temperature on Gr. 91 steel with different hea... WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch tensile/fracture test data for P92 nt material at -150 °C and a displacement rate of .00833 mm/s Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. For estimating the tensile properties a series of tests were carried out at room temperature on Gr. 91 steel with different hea... WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch creep test data for P92 ar material at 600 °C and a load of 450 N Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. Creep tests were carried out at temperatures in the range 550-650 ºC. WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch creep test data for P92 ar material at 650 °C and a load of 325 N Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. Creep tests were carried out at temperatures in the range 550-650 ºC. WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 0 O DIN-EU-SP-Standard-270 Small punch creep test data for P92 ar material at 650 °C and a load of 375 N Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. Creep tests were carried out at temperatures in the range 550-650 ºC. WEB DWN
Last updated: 7 Feb 2019 | Recent visits: 1 O DIN-EU-SP-Standard-270 Small punch creep test data for P92 ar material at 625 °C and a load of 375 N Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. Creep tests were carried out at temperatures in the range 550-650 ºC. WEB DWN